The plant adopts a crushing, grinding, and magnetic separation process designed for low-grade magnetite beneficiation.
The run-of-mine ore is first fed into a jaw crusher for primary crushing. Secondary crushing is completed by cone crushers working in closed circuit with vibrating screens, reducing the final product size to below 12mm.
To improve grinding efficiency and reduce energy consumption, the project integrates an HPGR system ahead of the ball mill. The grinding circuit consists of a ball mill and hydrocyclone cluster operating in closed circuit. Overflow slurry with 67% passing 200 mesh enters the magnetic separation stage.
A multi-stage wet magnetic separation process is applied to achieve an iron concentrate grade of 64.8% Fe with stable recovery performance.